Download as docx, pdf, or txt
Download as docx, pdf, or txt
You are on page 1of 1

MAGNETIC PARTICLE TEST REPORT

CUSTOMER: M/s. Shri Industries, Ekkatuthangal. CLIENT: M/s. FLSMIDTH Chennai


DATE: 04.09.2013

METHOD: Fluorescent AC Yoke with Water based Wet continuous method TEST PROCEDURE: SE 709 (ASME) REPORT NO :16810 INS.ORDER NO.: 20634 CURRENT USED: AC POWDER: Fluorescent Observation Remarks

DATE: 27/10/11 EQUIPMENT: SIMS Yoke SENSITIVITY: 2 mm Date : 03/12/10 Sl.No Specimen 1. Roller SL 05 Qty: 1 No Roller SL 06 Qty: 1 No Roller SL 07 Qty: 1 No Roller SL 08

2.

3.

4.

Qty: 1 No Customer Sign:

Group of air cracks observed from 3 locations of circumference Not Acceptable (Longitudinal 4 to 5 cracks in 3 location) Group of air cracks observed from 1 locations of circumference Not Acceptable (Longitudinal 4 to 5 cracks in 1 location) Group of air cracks observed in entire width (200mm) of roller at 3 locations of roller Not Acceptable circumference Deep transverse cracks noticed in entire width 200mm of roller at 3 locations of roller Not Acceptable circumference. Visually also noticed the same. Technical Level: II For Scaanray Metallurgical Services,
S.Balachandar S.Balu Alaganan V.Muthumanickam

Date: M. NAKKEERAN

L-II RT, UT, MT, PT. CHIEF OPERATIONS