Rev. 1 Scana Steel Stavanger as Quality no.

Quality group Quality

6006
Chemical analysis : C min max 0,22

UNALLOYED STEEL FOR CASTING

SE2

Si 0,60

Mn 0,50 1,20

S 0,030

P 0,030

Castings may also be delivered according to these comparable standards: NS-EN 10213-2 GP240GH W.nr.1.0619 DIN 1681 GS-45 W.nr.1.0446 ASTM A216 WCB SS 14 2172 ASTM A27 gr.65-35 JIS SCPH 1 NORSOK MDS-C02 BS 3100 AL1 NS 11645 Applications : SE2 is a standard construction steel with medium hardness and good weldability.

Minimum mechanical properties:


Yield Strength Tensile Strength Rm [MPa] Rp 0.2 [MPa] Elongation [%] Hardness [HB] Impact Charpy-V 20 C [J]

240

450-600

20

120-170

30

Heat treatment : Normalizing at 930-950 C cooled in air. On request SE2 may be Hardened and Tempered. Weldability : Excellent. Pre-heating at 100-200 C may be used on larger objects and under complicated welding conditions. Stress relieving (500-600 C) is recommended.
3

Specific weight: 7,8 g/cm . Pattern: Additional allowance for contraction: 2,0 %. 12,5 x 10 K -6 -1 13,3 x 10 K -6 -1 14,1 x 10 K
-6 -1

Coefficient of thermal expansion: 20-100 C: 20-300 C: 20-500 C: