G17CrMo5-5 (1.7357 ) Grade : Number: Standard: Classification: G17CrMo5-5 1.

7357 EN 10213 : 2007 steel castings for pressure purposes EN 10293 : 2005 steel castings for general engineering uses Ferritic and martensitic

Chemical composition % of the ladle analysis of grade G17CrMo5-5 (1.7357) For casting of ruling thickness < 28 mm, S =< 0.03 % (by mass) is permitted C 0.15 0.2 Si max 0.6 Mn 0.5 1 Ni max 0.4 P max 0.02 S max 0.02 Cr 11.5 Mo 0.45 0.65 V max 0.05 Cu max 0.3