STYROPAN XPS sheets

Technical Data Description


MINIMUM DENSITY THERMAL CONDUCTIVITY COEFFICIENT EN 12164 90 DAYS IN 10 C COMPRESSION STRENGTH EN 826 (value at yield limit or at 10% deformation) HYDRO-ABSORPTIVITY TEMPERATURE COEFFICIENT OF LINEAR EXPANSION Fire resistance EN 13501-1 DIN 4102 HAIR CRACKS RESISTANCE TO VAPOR PERMEABILITY (Air =1) MINIMUM / MAXIMUM LIMITS OF TEMPERATURE AT APPLICATION LENGTH DIMENSIONS WIDTH THICKNESSES EN 823 EN 822 mm mm 600 30, 50, 80 EN 12086 EN 12087 kp/cm % by volume mm/mK 2.5 1.5 max 0.07
0

Standard
EN 1602

Unit
kg/m W/mK kcal/mh C N/mm

Styropan
32 0.035 0.030 0.25

EUROCLASS E CLASS B2 None 100mij

C mm

-50 / +75 1250

Thickness of Extruded Polystyrene sheet - mm


30 50 80

R Value - mK/W
0.86 1.43 2.29

U Value - W/(mK)
1.17 0.70 0.44