Comparison Table between PP 651H (Sabic) and PPR R200P (Hyosung)

Properties
1)Resin Properties
Color
MRS classification
Melt flow rate @ 190C & 5.0kg
Melt flow rate @ 230C & 2.16kg
Density @ 23C
2)Mechanical Properties
Tensile Strength @ Yield
Tensile Elongastion @ Yield
Flexural Modulus (1% Secant)
Notched Izod Impact Strength @ 23C
Rockwell Hardness, R-Scale
3)Thermal Properties
Vicat softening point
Heat Deflaction temperature @
455KPa

Unit

Mpa
g/10 min
g/10 min
Kg/m3

Method

PP 651H
(Sabic)

Value
PPR R200P
(Hyosung)

ISO 9080
D 1238
D 1238
D 792

Natural
8
0.4
0.25
897

Grey
8
0.45
0.25
910

Mpa
%
Mpa
J/m
-

D 638
D 638
D 790A
D 256
D 785

28
13
900
220
93

27
400
850
300
60

C
C

D 1525A
D 648

135
80

130
90