Training Master

TRAINING SAMPLE ONLY


MACRO INSTRUCTION/REPORT SHEET [I.D: MR 1035]
MATERIAL: LOW CARBON STEEL
WELDING PROCESS: [MMA/SMAW]
9
1
2

3
4
7

#
1
2
3
4
5
6
7
8
9
10
11
12

DEFECT
Lack of sidewall fusion + 2 gas pores
Lack of sidewall fusion + slag
Lack of sidewall fusion + slag
Linear misalignment*
Lack of interun/sidewall fusion + slag
Lack of interun fusion + slag
Lack of sidewall fusion
Plate inclusions/laminations**
Arc strike***

SIZE

0.4 mm

ACCEPT/REJECT
Reject
Reject
Reject
Accept
Reject
Reject
Reject
Refer
Refer

EXCESS WELD METAL


EXCESS PENETRATION

COMMENTS:

* Also shows angular misalignment


** Acceptance depends upon specification requirements
*** Acceptance depends on specification requirements recommend blend smooth and
inspect