Interline 955 Performance Test Data For
Interline 955 Performance Test Data For
Interline 955 Performance Test Data For
Test Method
Specification Details
Typical Results
Cathodic
Disbondment
Cold Wall
Simulation
No blistering, cracking,
rusting and underfilm
corrosion following 696
hours exposure to cold
wall.
Condensation
No film defects
following 6000 hours
exposure.
No film defects
following 6000 hours
exposure.
Compressive
Strength
1 x 500m
821 kg/cm2
Elongation @
Break
1 x 500m
1.6% Elongation
1 x 500m
118 @ 1.05Kg
Immersion
Flexural
Properties
All representation and statements concerning the product(s) in this report are accurate to the best of our knowledge. Any
statements herein are not intended to be specific recommendations or warranties of any product, combination of products or
fitness for purpose
23/03/2005
www.international-pc.com
Page 1 of 2
Test Method
Specification Details
Typical Results
Hardness
(Barcol)
54 Barber Colman
Impact
Direct Impact
Resistance - 10.5 Joules.
Shear Strength
1 x 500m
385 Kg/cm2
Tensile Strength
1 x 500m
333 Kg/cm2
All representation and statements concerning the product(s) in this report are accurate to the best of our knowledge. Any
statements herein are not intended to be specific recommendations or warranties of any product, combination of products or
fitness for purpose
23/03/2005
www.international-pc.com
Page 2 of 2