Solve your UVA and UVB problems with

MBBT Organic Particles and Physical Filters (TiO2, ZnO)

New organic MBBT particles give possibilities to formulate cosmetically elegant


products with high UVA and UVB protection.

For Sun and Skin Care products the selection of UV protectors as particles gives two
benefits:

1) Truly skin caring non-penetrating actives


2) Protection of your other UV sensitive precious actives in the formulation on skin

What can be achieved?


Using ca 12 wt% particles of MBBT and ZnO:

 GAI-45ZS based Lotion


GranLux
SPF in vitro 26 +/- 2, UVA/UVB= 0,86

Using ca 12wt% particles of MBBT and TiO2

GAI-45TS based Cream


GranLux
SPF in vitro 49 +/- 3, UVA/UVB= 0,7

80
70
GAI-45TS Cream
60
50
MPF

40
GAI-45ZS Lotion
30
20
10
0
290 300 310 320 330 340 350 360 370 380 390 400
wavelength

SPF in vitro measured using 2 mg/cm2 of the sample on Vitro SkinTM

Oy Granula Ab Ltd. Phone: +358 5 2105200


Rautatienkatu 2 Fax: +358 5 2105225
FIN-48100 KOTKA e-mail: info@granula.com
Available MBBT containing products
GranLux® Application UV-Actives Composition
GAI-45 TS W/O emulsions; Creams and TiO2, MBBT
Lotions; High SPF Sun Care
GAI-45 ZS W/O emulsions; Lotions and ZnO, MBBT
Spray; Sun and Skin Care
GAI-45 TMBBT W/O emulsions; Sun Care TiO2, MBBT
GAI-45 ZMBBT W/O emulsions; Sun and Skin ZnO, MBBT
Care
GTI-45 TS O/W emulsions; Sun and Skin TiO2, MBBT
Care
GTI-45 ZS O/W emulsions; Sun and Skin ZnO, MBBT
Care
AB2-55 TMBBT various TiO2, MBBT
TG2-55 TMBBT various TiO2, MBBT
MMA-45 TMBBT W/O emulsions; Creams and TiO2, MBBT
Lotions; High SPF Sun and Skin
Care; Silicone and EO free

Formula: GAI-45ZS or GAI-45 TS High SPF Cream

INCI/Trade name Amount (%) Manufacturer

A) GranLux® GAI-45ZS or TS 27,0 Granula Ltd


Glycerine 3,0

B) Water 10,0
Nipagin M 0,1

C) Isononyl Isononanoate 20,0 Seppic

D) Water add to 100%


Parfume

1) Mix A at room temperature.


2) Prepare the water phase with preservative and add part of it (B) it to A. Mix ca 3-5 min until all
water has been taken up. The water will go in by diffusion, hydrate the polar parts and form the
liquid crystalline phase. The polar phase and the hydrophobic phase seem initially to be totally
separated but the water phase will be taken up by time and mixing.
3) Add to C to A+B while mixing. Viscosity goes down.
4) Add D to C+A+B slowly (during ca 5 minutes) while processing it well
(Ystral low speed ) for ca 5 min.