fill 11 min 3.2 5.1 E 7016 Kobelco N.A N.A N.A N.A N.A 32 - 19 90 - EP N.A 2280 N.A 45
fill 9 min 3.2 5.1 E 7016 Kobelco N.A N.A N.A N.A N.A 32 - 19 91 - EP N.A 1729 N.A 60
cap 10 min 3.2 5.1 E 7016 Kobelco N.A N.A N.A N.A N.A 32 - 19 91 - EP N.A 2074.8 N.A 50
Note :
3. Destructive Examination
TENSILE TEST CHARPHY TEST BEND TEST
Speciment No Size Area Load Tensile Stress Speciment Defect Remarks
Speciment No Location No Energy
Width (mm) Thicness (mm) (mm2) (kgf) (kgf/mm) (Mpa) (PSI) No Type Size
- - - - - - - - - - - - - - - - - - -
SEE ATTACHMENT - - - - - - SEE ATTACHMENT
- - - - - - - - - - - - - - - - - - -
- - - - - - - - - - - - - - - - - - -
- - - - - - - - - - - - - - - - - - -
4. Judgement
PASS RE-TEST FAIL