This table provides guidelines for preheat and interpass temperatures for welding various steel materials of different thicknesses. It specifies minimum and maximum temperature ranges for materials like quenched and tempered steel, high strength steel, and ordinary steel. Footnotes provide additional details about thickness limits and welding procedure specifications superseding the table.
This table provides guidelines for preheat and interpass temperatures for welding various steel materials of different thicknesses. It specifies minimum and maximum temperature ranges for materials like quenched and tempered steel, high strength steel, and ordinary steel. Footnotes provide additional details about thickness limits and welding procedure specifications superseding the table.
This table provides guidelines for preheat and interpass temperatures for welding various steel materials of different thicknesses. It specifies minimum and maximum temperature ranges for materials like quenched and tempered steel, high strength steel, and ordinary steel. Footnotes provide additional details about thickness limits and welding procedure specifications superseding the table.
Material2 Thickness Preheat and Interpass Temperature for welding (F˚)
Q&T or TMCP (mm) Minimum Maximum LR Grade 50 29 and Greater 200 300 XQ51 LR Grade 50 13-28 125 300 XQ51 LR Grade 50 Up to 12 60 300 XQ51 XQ47 64 and Greater 200 300 XQ47 28 to 63 150 300 XQ47 14 to 27 100 250 XQ47 Up to 13 50 200 HSS and Ordinary Steel 65 and Greater 2251 500 HSS and Ordinary Steel 38 to 64 1501 500 HSS and Ordinary Steel Up to 37 32 500 Steel Casting All 300 500 Footnotes: 1 = No preheat required for TMCP materials up to 55mm thick plate. 2 = The materials listed above are equivalent grades with 0.30% carbon maximum. 3 = A welding procedure specification supersedes Table I shown above and not limited to.