Top slab (Longitudinal)

Stress-tensile= 1.142 N/mm2


Section L= 1000 mm
D= 600 mm
Force-tensile= 685200 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 2166.64 mm2
Ast required on each face
16 mm dia @ 186 top & bottom
Ast provided= 16 mm dia @ 150 c/c Hence ..OK

Top slab (Transverse)


Stress-tensile= 0.148 N/mm2
Section L= 1000 mm
D= 600 mm
Force-tensile= 88800 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 280.7905 mm2
Ast required on each face
16 mm dia @ 1432 top & bottom
Ast provided= 16 mm dia @ 250 c/c Hence ..OK

Sea Side Wall (Longitudinal) ( TOP 1.0m depth)


Stress-tensile= 3.865 N/mm2
Section L= 1000 mm
D= 400 mm
Force-tensile= 1546000 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 4888.538 mm2
Ast required on each face
20 mm dia @ 129 on each face
Ast provided= 20 mm dia @ 100 c/c Hence ..OK

Sea Side Wall (Longitudinal) ( below 1.0m from top)


Stress-tensile= 0.396 N/mm2
Section L= 1000 mm
D= 400 mm
Force-tensile= 158400 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 500.8696 mm2
Ast required on each face
12 mm dia @ 452 on each face
Ast provided= 12 mm dia @ 200 c/c Hence ..OK

Land Side Wall (Longitudinal) ( TOP 1.0m depth)


Stress-tensile= 4.058 N/mm2
Section L= 1000 mm
D= 400 mm
Force-tensile= 1623200 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 5132.648 mm2
Ast required on each face
20 mm dia @ 122 on each face
Ast provided= 20 mm dia @ 100 c/c Hence ..OK

Land Side Wall (Longitudinal) ( below 1.0m from top)


Stress-tensile= 0.589 N/mm2
Section L= 1000 mm
D= 400 mm
Force-tensile= 235600 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 744.9802 mm2
Ast required on each face
12 mm dia @ 304 on each face
Ast provided= 12 mm dia @ 200 c/c Hence ..OK
Bottom slab (Longitudinal)
Stress-tensile= 0.017 N/mm2
Section L= 1000 mm
D= 400 mm
Force-tensile= 6800 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 21.50198 mm2
Ast required on each face
12 mm dia @ 10520 on each face
Ast provided= 12 mm dia @ 200 c/c Hence ..OK

Bottom slab (Transverse)


Stress-tensile= 0.336 N/mm2
Section L= 1000 mm
D= 400 mm
Force-tensile= 134400 N
Perm stress in steel=
0.55 x 500 x 1.15 = 316.25 N/mm2
Ast required= Force/perm stress= 424.9802 mm2
Ast required on each face
12 mm dia @ 532 on each face
Ast provided= 12 mm dia @ 200 c/c Hence ..OK