The document specifies the material, layering, construction techniques, and quality control for constructing a base course.
1) Crushed rock shall be used in layers not exceeding twice the maximum aggregate size, with each layer compacted to a thickness not less than the design thickness.
2) Layers shall be compacted thoroughly with a roller, measured for CBR and density, thickness, camber and level. Any nonconforming layers shall be reworked.
3) Quality control includes frequent measurement of CBR, thickness, and level, with measurement frequency adjustable depending on construction quality.
The document specifies the material, layering, construction techniques, and quality control for constructing a base course.
1) Crushed rock shall be used in layers not exceeding twice the maximum aggregate size, with each layer compacted to a thickness not less than the design thickness.
2) Layers shall be compacted thoroughly with a roller, measured for CBR and density, thickness, camber and level. Any nonconforming layers shall be reworked.
3) Quality control includes frequent measurement of CBR, thickness, and level, with measurement frequency adjustable depending on construction quality.
The document specifies the material, layering, construction techniques, and quality control for constructing a base course.
1) Crushed rock shall be used in layers not exceeding twice the maximum aggregate size, with each layer compacted to a thickness not less than the design thickness.
2) Layers shall be compacted thoroughly with a roller, measured for CBR and density, thickness, camber and level. Any nonconforming layers shall be reworked.
3) Quality control includes frequent measurement of CBR, thickness, and level, with measurement frequency adjustable depending on construction quality.
MATERIAL AND LAYER SPECIFICATION ,CONSTRUCTION TECHNIQUES AND QUALITY CONTROL
FOR CONSTRUCTION OF BASE COURSE
SPECIFICATION CONSTRUCTION TECHNIQUE QUALITY CONTROL
MATERIAL LAYER - Crushed rock shall be used. 1.CBR --------------- N.L.T. 80 % 1. Spread material in layers. Each compacted 1.Measurement of C.B.R layer shall not exceed twice the maximum - Material shall lie within 2.Compacted thickness size of the coarse aggregate. -Frequency of the following grading : - -Average compacted measurement ------- = 1/1000 sq.ft. thickness --- N.L.T. Design thickness 2. Check camber and level and make adjustment. COARSE AGGREGATE -Compacted thickness at any point---N.L.T. Design 3. Compact thoroughly with 8 to 10-ton smooth 2.Measurement of compacted thickness Size % Passing Thickness - 1/2" wheeled roller. -Frequency of 4.00" 100 3.Camber and level 4. Measure CBR and density of the compacted measurement ------ = 1/100 ft. 3.50" 90 - 100 -Deviation under 10 ft. layer. 2.50" 25 - 60 straight edge applied 1.50" 0 - 15 both parallel and at 5. Measure compacted thickness. 3.Measurement of camber and level 0.75" 0- 5 right angled to the centre line of the road---N.G.T. 3/8" 6. Measure camber and level.Compacted layer -Frequency of KEYSTONE -Level of the top which does not conform to the layer measurement ------ = 1/100 ft. Size % Passing most compacted specification shall be dug out,adjusted surface ----N.G.T. Specified level and recompacted. In consultation with the Quality 3/8" 100 ---N.L.T. Specified level - 1/2" Control Engineer, frequency of mea- 3/16" 85 - 100 surement can be changed depending 0.006" 10 - 30 on the quality and uniformity of the NOTE:- construction.
-Los Angles Abrasion ------ N.G.T. 50 % N.G.T. = Not Greater Than
-Crushing Value ------------- N.G.T. 30 % N.L.T. = Not Less Than -Flakiness Index -------------- N.G.T. 40 %