Zipper Pull Strength 80 N: Test Results Buyer Requirement

You might also like

Download as docx, pdf, or txt
Download as docx, pdf, or txt
You are on page 1of 1

Test Result Buyer

Requirement
Colour Change 4
Staining Acetate Cotton Nylon Polyester Acrylic Wool
4
Cross Staining - -

1. Colorfastness to Washing
Test condition: 40 deg with 4gpl ECE Phosphate ref. detergent &1gpl Sodium perborate with 10 steel balls)

2. Appearance after 3 washes


Test Method – ISO 6330:2012 (40˚C, Normal Cycle, Do not wash inside out, Line dry)

Observations : Buyer Requirement


Slight colour change of zipper observed
No removal of coating of puller or damage observed No Damage/Coating of
zipper/Puller
Functioning of zipper is proper
Appearance of garment is Satisfactory
Multifiber staining

Result Buyer
Requireme
nt
Colour change 4
Acetate Cotton Nylon Polyester Acrylic Wool
Staining 4
Cross Staining - -

3. Attachment strength: CRE type machine.

Product zipper

Test Results Buyer Requirement


Zipper Pull Strength 80 N

Slider Lock Strength 15 N