Professional Documents
Culture Documents
Birla Research Institute For Applied Sciences: Birlagram - 456331, Nagda (M.P.) INDIA
Birla Research Institute For Applied Sciences: Birlagram - 456331, Nagda (M.P.) INDIA
18 Brightness % - > 92 - -
19 Whiteness Berger 96 - 98 98
20 Yellow Index - - 5.95 - - 6.04 - 5.94
21 Reactivity % 15.8 - 11.5 16.7
22 Moisture % 6.8 10 9.13 7.52
Note : - The α-cellulose in recent SCHWEIGHOFER pulp is increase than to previous pulp and marginally less than to SAPPI pulp
- Compare to previous pulp,the lower values of S10 - S18 in recent Schweighofer pulp indicates presence of less degraded short
chain carbohydrate which ultimately affects on filterability.
- As compare to SAPPI and previous pulp sample, the viscosity of recent Schweighofer pulp is deteriorated, but still with in
acceptable range like other dissolving grade pulps.
Dr. R.K.Sharma