Visual Inspection Pipe Report

Name [Block capitals]____________ Signature_________________ Pipe Ident#___________

Code/Specification used____________Welding Process________ Joint type____________

Welding position___________ Outside ∅ and Thickness________ Date________________

Weld face

A B C

C D A

1
Pipe Root Face

A B C

C D A

2
Sentence Sheet for Pipe/Plate Inspection Report

Print full name ………………………………………………………………..

Specimen Number …………………….

Imperfections Code or specification reference Sentence


Face imperfections reported
Maximum
Imperfection types Maximum value allowed by Code section or Accept or
or total length code Table No reject
1 2 3 4
Excess weld metal (height)
Toe blend/inter-run blend
Incomplete filling
Slag inclusions
Undercut
Surface porosity
Cracks
Lack of fusion
Arc strikes
Mechanical damage
Misalignment

Root Imperfections
Misalignment
Penetration (height)
Lack of root penetration
Lack of root fusion
Root concavity
Root undercut
Cracks
Porosity
Burnthrough

This pipe/plate* has been examined to the requirements of [code/specification]..................…...


and is accepted/rejected* accordingly. [*Delete whichever is not applicable]

Signature..............….................................…….…
Date...............................