Matarbari Area, Maheshhali Upazila, Cox's Bazar District, Chittagong Division, Bangladesh

Adjustment of Concrete Mix Proportion for Batching Plant


Date of Casting : Time

Concrete class : mortar Lab.Ref .No

Component of structure :

Location : Foundation & Basement slab Brand of Cement : AM

Supplier of concrete No.02 BP Water/Cement Ratio :

Requirement quality : 1.0 m3 Water Content : 290 kg/m3

Sand / Aggregate Ratio ( S/A ) : 0.0 % Cement Content : 553 kg/m3

F/A= 1690 kg/m3 C/A= 0 kg/m3 Density of Admixture (SIKA ) : 1.09

Design Slump : mm Recommended Dosage 0.00 % by wt of cement

1.Moisture Content Test:

Moisture Content Determination


Water Absorption
Weight of
Type of Materials Wet Weight Dry Weight Moisture Content
Water
g g g % %

4.75 mm Fine Aggregate 0.0 0.0 0.0 1.50

20 mm Coarse Aggregate 0.0 0.0 0.0 0.51

2. Mix Batching plant

SSD- Basis (kg) per m³ Computation for free moisture (Kg/m3) Corrected Weight (Kg/m3)

Cement 553 553

F/A 1690 = 1690

C/A 0 = 0

Admixture 0.00 = 0.00

Water 290 Σ 0.0 290 - 0.0 = 290

Lab Manager QA/QC SUMITOMO Engineer's Representative


Sinohydro POSCO Matarbari JV Consultants