2
C35R ( 1.1180 )
Grade : C35R
Number: 1.1180
EN 10277 - 5 : 2008 Bright steel products. Technical delivery conditions. Steels for quenching and
tempering
Standard:
EN 10083 - 2 : 2006 Steels for quenching and tempering. Technical delivery conditions for non alloy
steels
C Si Mn Ni P S Cr Mo
0.32 - 0.39 max 0.4 0.5 - 0.8 max 0.4 max 0.03 0.02 - 0.04 max 0.4 max 0.1
M e c ha nic a l pr ope r t ie s of gr a de C3 5 R ( 1 .1 1 8 0 )
Rp0.2 0.2% proof strength (MPa) (+C) 510 420 320 300 270
+20°
KV - Impact energy (J) (+QT)
35
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=183 1/3
3/6/2014 C35R / 1.1180 - steel equivalent, mechanical properties, chemical composition
A - Min. elongation at fracture (%) (+C) 6 7 8 9 9
P r ope r t ie s of gr a de C3 5 R ( 1 .1 1 8 0 )
Weldability: It can be welded quite well without any precautions.
Hardenability: Low hardenability; core quenching in water till a diameter of 12-15 mm; as far as bigger diameters are concerned, it
hardens only till a certain depth, inversely proportional to diameter, like all non-alloy steels with medium-high carbon content.
Equiva le nt gr a de s of gr a de C3 5 R ( 1 .1 1 8 0 )
Warning! Only for reference
USA Germany France England Italy Spain Inter
- DIN,WNr AFNOR BS UNI UNE ISO
1035 C35 XC38H1u 080M36 C35 C35K1 C35M2
Cm35 F1135(1)
M e c ha nic a l pr ope r t ie s
M e c ha nis c he Eige ns c ha f t e n
Ca r a c t e r is t ique s m e c a nique s
R eH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
R m Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc
He a t t r e a t m e nt c ondit ions
+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=183 2/3
3/6/2014 C35R / 1.1180 - steel equivalent, mechanical properties, chemical composition
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated
Chemical composition of C35R (1.1180). Equivalent grades of C35R (1.1180). Standards of C35R (1.1180).
Properties of C35R (1.1180). Hardness of C35R (1.1180). Strength of C35R (1.1180). Elongation of C35R (1.1180).
© 2011- 2014 All rights reserved. The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=183 3/3