Professional Documents
Culture Documents
European Steel and Alloy Grades: Alloy Standards Search About Us EN 10277-2 EN 10162
European Steel and Alloy Grades: Alloy Standards Search About Us EN 10277-2 EN 10162
YOU HERE: Steel numbers -> Number 1.05XX OR Steel and cast iron standards -> / EN 10277-2 / EN 10162
S355J2C ( 1.0579 )
Grade : S355J2C
Number: 1.0579
EN 10277 - 2 : 2008 Bright steel products. Technical delivery conditions. Steels for general
Standard: engineering purposes
EN 10162 : 2003 Cold rolled steel sections. Dimensional and cross-sectional tolerances
max 0.2 max 0.55 max 1.6 max 0.03 max 0.03 max 0.55
M e c ha nic a l pr ope r t ie s of gr a de S 3 5 5 J 2 C ( 1 .0 5 7 9 )
Rp0.2 0.2% proof strength (MPa) (+C) 520 450 350 335 315
P r ope r t ie s of gr a de S 3 5 5 J 2 C ( 1 .0 5 7 9 )
Weldability: This steel grade is generally suitable to welding.
Equiva le nt gr a de s of gr a de S 3 5 5 J 2 C ( 1 .0 5 7 9 )
Warning! Only for reference
Germany England Italy
DIN,WNr BS UNI
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=146 1/2
3/6/2014 S355J2C / 1.0579 - steel equivalent, mechanical properties, chemical composition
St52-3N 50D8 Fe510D
M e c ha nic a l pr ope r t ie s
M e c ha nis c he Eige ns c ha f t e n
Ca r a c t e r is t ique s m e c a nique s
R eH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
R m Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc
He a t t r e a t m e nt c ondit ions
+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated
Chemical composition of S355J2C (1.0579). Equivalent grades of S355J2C (1.0579). Standards of S355J2C (1.0579).
Properties of S355J2C (1.0579). Hardness of S355J2C (1.0579). Strength of S355J2C (1.0579). Elongation of S355J2C
(1.0579).
© 2011- 2014 All rights reserved. The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=146 2/2