Special Structural Repair Work at Slab.
S. No. DESCRIPTION QTY
1 Chipping of loose concrete/Plaster(0-20mm thick) by mechanical and manual means
to expose internal reinforcement and stacking of debris within a lead of 30 m. 350.00
2 REBARRING: Providing and fixing Re-bar with Hilti HY-200/RE-500 or equivalent and
complete as per the manufacturer's specification for standard depths.
STEEL 8mm 20.00
Scraping of rust from surface of reinforcement. Providing and applying rust remover
coating over the exposed surface. Zinc coating Providing and applying anti-
3 corrosive zinc coating on existing reinforcement. 350.00
Providing and applying polymeric based bonding agent over the surface before
placing concrete. (Nito Bond)
Providing and applying polymer modified concrete. (Micro Concrete BASF ,
SIKA,Fosroc) 100.00
Shotcrete: Providing and laying Shotcrete/guniting is the process of repairing
Concrete Workof the reason.Guniting was a method of early origin in the US, where
4 the method is defined as the process of spraying a mix or mortar or concrete to a
surface of application with the help of a spray gun. This method makes use of a spray
gun and hence the process was named as Guniting was a method of early origin in
350.00
the USA. average thickness 25-40 mm mix of 1:3 (1 cement : 3 sand) with
waterproofing compounds.(Recron Or MasterPell 777)

Shotcrete is also applied with steel fibers that will be applied like a replacement of
5 welded wire mesh. It allows greater flexural strength, ductility and toughness.with 350.00
welded mesh (10 gages, 100 mm x 100 mm)

Slab And Beam Strenghtening


Nozzle Fixing : Drilling Holes of 12mm dia, upto 100mm deep holes in structural
members at the intervals of 500mm in staggered manner or along the crack or as
1 directed by the consultants in RCC structural element including cleaning of the holes 100.00
by air blower and Inserting 12mm dia.
Epoxy Injection: Supply and apply a two part, low viscosity, moisture insensitive
injection-liquid, based on high strength epoxy resin.
Product: Sikadur®-52 LP (IN)/Equivalent
2 Mixed Density: 1.1 kg/ltr. at 270C 100.00
(Sika/Basf/Fosroc/Ecmas)

SUB TOTAL

TERMS AND CONDITIONS:


1. 50% Mobilization Advance.

2. Monthly bill submission and payment to be made within 2-3 days.


3. Water and Electricity to be provided by client free of cost at site.
4. Final billing will be based upon actual measurements to be done at the site.
5. Taxes Extra as applicable.
Solutions"
Solutions.
Vihar, New Delhi-110063
302880,9211661909

12/6/2021

ab.
UNIT Rate Amount

Sqft 20 7000

Nos 380 7600

Sqft 35 12250

Kg 68 6800

Sqft 75 26250

Sqft 25 8750

Nos 250 25000

Nos 550 55000

148,650.00