Void Space Condition Report

VESSEL: DATE:
SPACE:
Rating Structure 3)
Notes:Enter any relevant info re structure
or coating condition improvement with

Deformation
Inspection 1)

Corrosion 5)
Area

ref. to last class hull survey report. All


Item

Fractures
Coating 4)
observations like cracks, bendings etc to
be examined and status entered as
remark

Bottom plating with stiffeners


Side plating with stiffeners (P)
Side plating with stiffeners (S)
frames,stiffen.,girders,stringers etc.)

Top plating with stiffeners


Longitudinals girders
Structure (incl. plates

Transverse girders
Longitudinal bulkheads (P)
Longitudinal bulkheads (S)
Transverse bulkhead (Fore)
transverse bulkhead (Aft)
Web frames
Drainage holes

Ladders & Platforms


Bilge wells & piping
Fire extinguishing piping
Outfitting

Sounding piping
Steam piping (heating)
Fuel Oil piping
Air & Ventilation piping
Lighting
Vent Heads (internal)
GEN. COND. OF
COATING 2)
GOOD
FAIR Inspected By:
POOR
REMARKS
1) Mark as follows: Y: Inspected / N: Not inspected / NA: Not applicable
2) Mark with X
3) Mark with X if found and give explanation in Notes
4) Mark Rating as follows: (see Assessment scale on next page)
1-Coating breakdown <=0.1% (GOOD)
2-Coating breakdown 0.1%<2% (GOOD)
3-Overall coating breakdown 2%<20% Or local coating breakdown at the edges of stiffeners and weld
connections >=20% but less as defined for poor condition (FAIR)
4-Overall coating breakdown 20%<50% (POOR)
5-Overall coating breakdown >50% (POOR)
5) Mark Rating as follows: (see Assessment scale on next page)
1- Minor spot rust <=0.1%
2- Light rust 0.1%<2%
3- Light rust 2%<20% and hard scale <10%
4- Hard scale >10%
5- Hard scale >20%