Download as pdf or txt
Download as pdf or txt
You are on page 1of 7

AEROSOL SPRAY FORMULATIONS E BOOKS

AEROSOL
SPRAYS
FORMULATIONS

E – BOOKS
AEROSOL SPRAY FORMULATIONS E BOOKS

Allrights of this publications belongs to

SOLVERCHEMBOOKS
AEROSOL SPRAY FORMULATIONS E BOOKS

HAIR CARE
PRODUCTS
SPRAY

FORMULATIONS

E – BOOKS
CONTENT

AEROSOL HAIR SPRAY

FORMULATIONS AND MANUFACTURING PROCESS

1 – AEROSOL HAIR SPRAY


FORMULATION AND PRODUCTION PROCESS – 1

2 – AEROSOL HAIR SPRAY


FORMULATION AND PRODUCTION PROCESS – 2

3 – AEROSOL HAIR SPRAY


FORMULATION AND PRODUCTION PROCESS – 3
AEROSOL
HAIRSPRAY
PRODUCTION PROCESS – 1

NO CAS W/W
INGREDIENTS NUMBER
1 POLYVINYLPYRROLIDONE K 30 2

2 GLYCERINE 0.250

3 ETHYL ALCOHOL 45

4 D - PANTHENOL 0.250

5 PERFUME 0.250

6 DEINOIZED WATER 52.250

TOTAL 100

PROCESS:Charge ethyl alcoholin the process tank. Start to mix. Add


polyvinylpyrrolidonewhile mixing. Dissolve polyvinylpyrrolidone in the
ethyl alcohol completely. Add the rest of ingredients and mix well.
Continue to stirr until mixture is homogenous. Homogenous is enough.
Process is completed.

NOTE: For production of 500 ml aerosol spray is used 200 g above


product and 270 – 275 g LPG gaseous ( Propellant )

** 1 **
AEROSOL
HAIRSPRAY
PRODUCTION PROCESS – 2

NO CAS W/W
INGREDIENTS NUMBER
1 POLYVINYLPYRROLIDONE K 30 2.250

2 DIMETHICONE 0.250

3 GLYCERINE 0.250

4 ETHYL ALCOHOL 50

5 D - PANTHENOL 0.250

6 PERFUME 0.250

7 DEINOIZED WATER 46.750

TOTAL 100

PROCESS:Charge ethyl alcohol in the process tank. Start to mix. Add


polyvinylpyrrolidonewhile mixing. Dissolve polyvinylpyrrolidone in the
ethyl alcohol completely. Add the rest of ingredients and mix well.
Continue to stirr until mixture is homogenous. Homogenous is enough.
Process is completed.

NOTE: For production of 500 ml aerosol spray is used 200 g above


product and 270 – 275 g LPG gaseous ( Propellant )

** 2 **
AEROSOL
HAIRSPRAY
PRODUCTION PROCESS – 3

NO CAS W/W
INGREDIENTS NUMBER
1 POLYVINYLPYRROLIDONE K 30 2

2 ISOPROPYL ALCOHOL 45

3 PERFUME 0.150

4 DEINOIZED WATER 52.850

TOTAL 100

PROCESS:Charge isopropyl alcohol in the process tank. Start to mix.


Add polyvinylpyrrolidonewhile mixing. Dissolve polyvinylpyrrolidone in
the isopropyl alcohol completely. Add water and perfume during
constant mixing. Continue to stirr until mixture is homogenous.
Homogenous is enough. Process is completed.

NOTE: For production of 500 ml aerosol spray is used 200 g above


product and 270 – 275 g LPG gaseous ( Propellant )