Samples for Slit Tensile Tests 3 300x150 Cube Each (27 cubes)
Required % Fine Coarse
Cement Alkaline Activated Water Content
S/No. Volume, cubic-m Cement Replacement Content (kg) Kaolin (kg) (kg) Aggregate, Aggregate
Content (kg) of Cement (kg) (kg)
1 0.0159043128087983 4.5 0.0 4.5 0.000 2.9 8.9 17.8
2 0.0159043128087983 4.5 2.5 4.3 0.111 2.9 8.9 17.8
3 0.0159043128087983 4.5 5.0 4.2 0.223 2.9 8.9 17.8
4 0.0159043128087983 4.5 7.5 4.1 0.334 2.9 8.9 17.8
5 0.0159043128087983 4.5 10.0 4.0 0.445 2.9 8.9 17.8
6 0.0159043128087983 4.5 12.5 3.9 0.557 2.9 8.9 17.8
7 0.0159043128087983 4.5 15.0 3.8 0.668 2.9 8.9 17.8
8 0.0159043128087983 4.5 17.5 3.7 0.779 2.9 8.9 17.8
9 0.0159043128087983 4.5 20.0 3.6 0.891 2.9 8.9 17.8
Totals= 36.1 4.008 26.1 80.2 160.3
Coarse
Cement (kg) Alkaline Activated Water Content Fine Aggregate
Kaolin (kg) (kg) Aggregate (kg) (kg)
Quantities 59.0 6.6 42.6 131.2 262.4
NaOH
1 0.0
2 2.5 0.071 kg
3 5.0 0.14175
7.5 0.2835
10.0 0.567
12.5 1.134