ROCORR MFL-C SERVICE

IN-LINE HIGH-RESOLUTION METAL LOSS


AND NARROW AXIAL FEATURE ANALYSIS

A precise and detailed identification of metal KEY ADVANTAGES


loss and, in particular, axial-oriented anoma- • Accurate metal loss characterization in welded and
specifically in seamless pipeline by extra high sensor
lies like narrow corrosion, gouging, channeling,
density and high sampling rate
crack-like features and preferential seam weld • Lifetime integrity management supported by full recording
corrosion is a basic element for the integrity of the raw inspection data
management of oil and gas pipelines. • Largest tool fleet on the market ensuring global tool
availability and flexibility
Our RoCorr MFL-C service is a reliable and ef- • High-quality service with certified processes (API 1163),
fective means of managing your pipeline integ- personnel qualification (ASNT) and equipment (CE, ATEX)

rity especially for concerns related to the long


seam (e.g. pre-1970 ERW). All aspects from the
inspection request to the final report are cov-
ered with the flexibility to choose from various
service options.

THE SOLUTION
A circumferential induced magnetic field generates an
optimum response from any volumetric axial-oriented
pipeline feature. Combining this with our unique sensor design
makes ROSEN’s Circumferential Magnetic Flux Leakage
Technology most suitable to reliably and effectively detect
and characterize challenging metal loss features such as
Selective Seam Weld Corrosion (SSWC). When combined with SERVICE OPTIONS
SSWC susceptibility analysis based on material properties and All aspects from the inspection request to the final report are
environmental conditions, this enables the differentiation of covered with the flexibility to choose from various service
SSWC from ‘general’ corrosion that happens to be coincident options.
with the longitudinal seam weld. This approach relies on an • Cleaning – operational and pre-inspection
advanced evaluation review of the in-line inspection (ILI). • Speed Control – inspection at high flow rates
Our well–structured, certified data evaluation process • XYZ – route mapping and strain assessment
enables ROSEN’s data analysts to provide the required high • Multi-Diameter – pipelines with varying diameter
quality assessment on-time. • Combo – multiple inspection technologies in one run
Our reporting software ensures easy data visualization and • Offshore – long distance and high pressure
facilitates the broad use of inspection results. • Post-ILI – data alignment and combined evaluation
• Integrity Assessments – RBI, FFP, CGA
• NIMA – versatile asset integrity software suite

www.rosen-group.com
ROCORR MFL-C SERVICE
IN-LINE HIGH-RESOLUTION METAL LOSS AND NARROW AXIAL FEATURE ANALYSIS

TECHNICAL SPECIFICATIONS
Standard Operating Specifications Metal Loss Feature Classification
Tool sizes available 6" - 56" All reported metal loss features are classified according to
Pipeline product Gas or liquids the dimensions shown in the following Pipeline Operators’
Product temperature range 0 °C - 65 °C (14 °F - 149 °F) Forum (POF) specification graph.
Maximum operating pressure 15 MPa (2,175 psi)
25 MPa (3,625 psi) optional A = wall thickness or 10 mm (0.39”), whichever value is greater

Operating speed range Up to 5.0 m/s (11.2 mph)

Width/A

Circumferential grooving
Product flow range Up to 11 m/s (24.6 mph)
8
Minimum pipeline bend radius 1.5D

Circumferential slotting
Wall thickness range 4 - 25 mm (0.15" - 1.0") 7

Maximum operating time 400 hours


6
Maximum inspection length 800 km (500 miles)
5 General
Note: Please contact ROSEN for conditions outside of these specifications.
*Fitted with optional speed control system
4

2 Pitting Axial grooving


Location and Orientation Capabilities
Axial position accuracy from reference marker 1:1000 1
1 m on 1,000 m marker distance Axial slotting
1 ft. on 1,000 ft. marker distance
1 2 3 4 5 6 7 8
Axial position from closest weld ±0.1 m (±4") Pinhole Length/A
Accuracy of circumferential position ±5°
The axial positioning accuracy specified is given at 90 % certainty and is based on Wall Thickness Detection
following conditions: ±1 mm (± 0.04”) or ±0.1t, whichever value is greater at
1. D
 istance between upstream (u/s) and downstream (d/s) marker/reference point <
2,000 m (6,500 ft.). 80 % certainty
2. A
 ctual aboveground distance to both u/s and d/s marker/reference points have been t = wall thickness
measured and correlated.
3. Marker points are placed correctly according to respective ROSEN marker specification.

Performance Specifications

General Pitting Axial Grooving Axial Slotting*


Depth at POD = 90 % 0.15 t 0.15 t 0.10 t 0.20 t
Depth sizing accuracy at 80 % certainty ±0.15 t ±0.19 t ±0.15 t ±0.15 t
Length sizing accuracy at 80 % certainty ±15 mm (0.59") ±12 mm (0.47") ±15 mm (0.59") ±15 mm (0.59")
Width sizing accuracy at 80 % certainty ±15 mm (0.59") ±15 mm (0.59") ±15 mm (0.59") ±8 mm (0.31")
*Valid for axial slotting feature width > 1 mm (0.039”)
Abbreviations: POD = Probability of Detection; t = wall thickness

Remarks and Features


• API 1163 compliant services
• CE and ATEX certification available
• Tailored solutions with different specifications upon request: multiple tool sizes or multi-diameter tools, higher pressure rating
• Specifications are subject to change due to specific requirements or tool configurations

© 2022 ROSEN Swiss AG. All Rights Reserved.


Obere Spichermatt 14 · 6370 · Switzerland · Phone: +41-41-618-0300 · rosen-stans@rosen-group.com
RoCorr-MFL-C_SF_EN_22.1.1_A4
Entire content is for general information purposes only and is believed to be accurate. ROSEN will not accept any liability in connection with the content. This
limitation applies to all loss or damage of any kind, including but not limited to, compensatory, direct, indirect or consequential damage, loss of income or profit,
loss of or damage to property and claims by third party.

www.rosen-group.com

You might also like