PIPING PWHT REQUIREMENT

ASME B31.3 ASME B31.4 ASME B31.8


REMARKS
(2010 edition) (2006 edition) (2010 edition)
MATERIAL
Hard
Para. 331.1.1 Table 1 P No Para. 434.8.9 Para. 825.2
(BHN)

Carbon Steel >20 mm(3/4") THK 1 -

Alloy Steel > 20 mm(3/4") THK,


3 225
Cr ≤ 1/2% >SMTS 71 ksi

Alloy Steel >13 mm(1/2") THK,


4 225
1/2%< Cr ≤ 2% >SMTS 71 ksi

Alloy Steel >13 mm(1/2") THK, 5A,5B,


241
2-1/4% ≤ Cr ≤ 10% >3% Cr or C>0.15% 5C
High Alloy Steel >32 mm(1-1/4")
(Martensite), All 6 241 THK
A240 Gr.429 (Exceed 1-1/4")
>32 mm (1-1/4")
High Alloy Steel
None 7,8 - ☞ Min. Preheating THK for CS
(Ferritic, Austenitic)
93℃ for CS (Exceed 1-1/4")
32 mm(1-1/4") ~
Nickel Alloy Steels >20 mm(3/4") THK 9A,9B - 38 mm(1-1/2")
may be exempted

Cr-Cu / Duplex SS / 27Cr Steel All 10/10H/10I -

11A SG 1/
8Ni, 9Ni / 5Ni Steel >51 mm(2") THK -
11A SG 2

Alloy Steel 9Cr-1Mo-V All 15E _

Zr R60705 All 62 _

# Note : 1. Fabrication, Assembly, and Erection에 적용

2. 원자재인 경우(Pipe, Fitting, Flange등)에는 orginal code and standard에 따라서 열처리 (즉, ASTM, API 등)

3. NACE MR 0175 material인 경우에는 orginal code and standard에 추가하여 상기 사항 적용

4. SMTS means Specified Min. Tensile Strength.

C:PWHT req as per Code(PWHT) 1 of 1 Printed Date : 2012-12-10

You might also like