A Floor
1 Screed Indoor Compressive Strength 4 - 6 N/mm2 6 - 10 N/mm2 Uzin Screed Mix
Adhesion Strength 0,8 N/mm2
2 Screed Outdoor (Carport/terrrace/balcony/deck) Uzin RC 25
Compressive Strength 16 N/mm2 6 - 10 N/mm2
3 Perekat Keramik / HT area kering / lembab Adhesion Strength > 0,5 N/mm2 > 0,5 N/mm2 Uzin Bond
Adhesion Strength > 0,5 N/mm2 > 0,5 N/mm2 Uzin Bond Plus
4 Perekat Keramik / HT area terendam / Pond / Pool
Tahan air berkaporit
B Wall
0,3 - 0,5 N/mm2
1 Adhesion Strength 0,4 - 0,5 N/mm2 Uzin TB 20
Perekat bata ringan (umur 28 hari)
Adhesion Strength 0,2 - 4,0 N/mm2
2 Perekat Bata Merah (trasram) N/A N/A
& kedap air
3 Plasteran Bata Ringan Adhesion Strength 0,2 - 0,25 N/mm2 0,2 N/mm2 Uzin Plaster Mix
Adhesion Strength 0,2 - 4,0 N/mm2
4 Plasteran Bata Merah (Trasram) N/A N/A
& kedap air
Adhesion Strength 0,3 - 0,5 N/mm2 Uzin SC50 (Interior)
5 Acian Bata Ringan / Merah 0,3 - 0,5 N/mm2
Compressive Strength 10 - 12 N/mm2 Uzin SC75 (Exterior)
6 Perekat Keramik / HT area kering / lembab dengan Adhesion Strength > 0,5 N/mm2 > 0,5 N/mm2 Uzin Bond
tebal s/d 9mm
Perekat HT / Batu Alam area kering / lembab dengan
7 Adhesion Strength > 0,5 N/mm2 > 0,5 N/mm2 Uzin Bond
tebal s/d 10 - 20 mm
Adhesion Strength > 0,5 N/mm2 > 0,5 N/mm2 Uzin Bond Plus
8 Perekat Keramik / HT area terendam / Pond / Pool
Tahan air berkaporit
C Miscelaneous
1 Grouting Nat Keramik / HT area kering / lembab N/A N/A Uzin Tile Grout
Abrasive Resistance 102 N/mm2
2 Grouting Nat Keramik / HT area basah / Pond / Pool N/A N/A
Compressive Strength 30 N/mm2
D Beton Instant
1 Beton Instant K-175 UZIN K-175
2 Beton Instant K-350 UZIN K-350