Download as pdf or txt
Download as pdf or txt
You are on page 1of 4

ROBOND™ L Water-borne

Laminating Adhesives
North American Product Guide
ROBOND™ L Water-borne Laminating Adhesives
North American Region

Product Guide Unique Benefits and Features of Ease of Use


Dow offers a broad line of water-borne Acrylic Water-borne Technology • Processing advantage (line speeds in
dry bond laminating adhesives. Current • Supply chain benefits excess of 900 feet/minute)
products are joined by new technology, • Acrylic waterborne technology provides • Run speeds limited only by dryer capacity
and uncommon support offers solutions to high shear strength enabling immediate • Easy handling and mixing
a wide range of adhesive needs. slitting and fast delivery (see Figure 1) • Delivered ready-to-use without dilution
• Wide range of end use applications • Slit and ship the same day – • Long pot life compared to PUD/NCO
• Technical expertise and support – Reduced work in process water-borne adhesives
• Full pilot coating capabilities to test your – Reduced inventory costs • Can be used for printing and laminating
application needs – Decreased working capital costs in-line
• Economical and planet-friendly • Delivered ”machine ready” • Wide variety of film and foil structures for
technology – No dilution required varied end-use applications
The water-borne products find util- – No solvents • Runs on existing solvent-based
ity in general purpose snack and bottle – Reduced labor costs laminating equipment
label applications as well as applications • For specific handling guidelines, refer • Fast slit-to-ship turnaround
that require heat, moisture and product to our brochure “ROBOND™ L-Series • Manufacturing flexibility
resistance, such as microwaveable food Acrylic Adhesives Pre-trial Guidelines”
packaging and boil-in-bag structures. For (form number 500-14701)
your specific application needs, please Figure 1: Shear Strength Properties
consult your Dow representative. Health and Safety Benefits 100% = Shear Required for Immediate Slitting
105%
• Acrylic emulsions are free of 100% 104% 103%
95%
organic solvents (VOCs), offering you and
your customer:
Lap Shear

– No retained solvents due to adhesive


– Safer work environment
– No solvent exposure due to adhesive
– Reduced flammability hazards (possible
insurance savings)

Environment SB1 SB2 SB3 WB1


Adhesive Type
• Environmentally friendly adhesive system
• Non-hazardous health and safety rating ROBOND™ L water-borne adhesive products
have high shear strength for immediate slitting
• Water based means reduced
dependency on oil feedstocks
• Reduced pollution
• “Green” technology

™Trademark of The Dow Chemical Company (“Dow”) or an affiliated company of Dow


Table 1: Product Range: Quick Use Guide and Performance Profile
ROBOND™ L Component L-90M L -100 L -148 L - 330
Coreactant Alone or CR 9-101 CR 9-101 Alone or CR 9-101 CR 9-101
Mix Ratio 100:2 100:2 100:2 100:2
Film/Foil X x x
Metallized Films X X x x
Film/Film X x x x
EVA Films X X x x
White PE/EVA X X x x
Product Resistance Fair Acceptable Better Best
Pasteurization of Film Laminates Not Recommended Acceptable Acceptable Best
Pasteurization of Foil Laminates Not Recommended Acceptable Acceptable Best
Heat Resistance Fair Better Better Best
FDA Status* 175.105 175.1395 175.1395 175.1395

*The FDA information above relates specifically to the product mentioned. The FDA information is accurate and reliable as of the date of publication. Customer’s use of the adhesive may affect FDA compli-
ance. Customers are responsible to make their own judgment regarding suitability of the product for the end-use application. We cannot guarantee the on-going FDA compliance status of any individual
product; therefore, we recommend that customers periodically verify status. Refer to individual technical data sheets or consult your Dow representative for more detailed FDA compliance information.
For more information about Dow, visit www.dow.com/about, or contact a Dow representative at www.dow.com/contact.

NOTICE: No freedom from infringement of any patent owned by Dow or others is to be inferred. Because use conditions and applicable laws may differ from one location to another and may change
with time, Customer is responsible for determining whether products and the information in this document are appropriate for Customer’s use and for ensuring that Customer’s workplace and disposal
practices are in compliance with applicable laws and other government enactments. The product shown in this literature may not be available for sale and/or available in all geographies where Dow is
represented. The claims made may not have been approved for use in all countries. Dow assumes no obligation or liability for the information in this document. References to “Dow” or the “Company”
mean the Dow legal entity selling the products to Customer unless otherwise expressly noted. NO WARRANTIES ARE GIVEN; ALL IMPLIED WARRANTIES OF MERCHANTABILITY OR FITNESS FOR A
PARTICULAR PURPOSE ARE EXPRESSLY EXCLUDED.
THIS INFORMATION IS OFFERED IN GOOD FAITH FOR YOUR CONSIDERATION, BUT WITHOUT GUARANTEE OR WARRANTY (EXPRESS OR IMPLIED), AS ANALYTICAL CONDITIONS AND
METHODS OF USE OF THE INFORMATION AND MATERIALS DESCRIBED HEREIN MAY VARY AND ARE OUT OF DOW’S CONTROL. ALTHOUGH THIS INFORMATION IS BASED ON DATA DOW
BELIEVES TO BE RELIABLE AND ACCURATE, WE DO NOT INTEND FOR YOU TO USE, AND YOU THEREFORE SHOULD NOT CONSTRUE, THE CONTENTS OF THIS DOCUMENT AS BUSINESS,
TECHNICAL OR ANY OTHER FORM OF ADVICE. WE RECOMMEND YOU DETERMINE THE SUITABILITY OF THE INFORMATION AND MATERIALS DESCRIBED HEREIN BEFORE ADOPTING OR
USING THEM ON A COMMERCIAL SCALE. DOW ASSUMES NO LIABILITY IN CONNECTION WITH THE USE OF THIS INFORMATION.

This document is intended for use in North America.


© 2021 The Dow Chemical Company

Trademark of The Dow Chemical Company (“Dow”) or an affiliated company of Dow



901-104-01-0921 SMG
SMG 12797

You might also like