Professional Documents
Culture Documents
SMA 13mm
SMA 13mm
SMA mixes having the proportions (85% RAP, 15% virgin Aggregates by using ANT
rejuvenator of 0.01%) and different trial proportions were done in the laboratory for the
determination of volumetric and strength properties.
100
90
80
% of Passing
70
60
50
40
30
20
10
0
0.1 0.1 0.2 0.4 0.8 1.6 3.2 6.4 12.8 25.6 51.2