Thermanit - 2535R. Aporte Manaurita XM

You might also like

Download as pdf or txt
Download as pdf or txt
You are on page 1of 1

Thermanit 25/35 R

GTAW welding rod

Classifications EN 12072 Mat. No.


W Z25 35 1.4853

Characteristics Resistant to scaling up to 1050 °C (1922 °F).


and field of use For joining and surfacing work with matching/similar
heat resistant cast steel grades

Marks 1.4853 / 25/35 R

Materials TÜV-certified parent metal


GX40NiCrSiNb35-25 (1.4852)

Typical analysis C Si Mn Cr Ni Nb
in % 0.42 1.0 1.8 26.0 35.0 1.3

Creep and stress In the range of matching cast steel grades


rupture properties

Mechanical proper- Heat- Yield strength Yield strength Tensile Elongation Impact values
ties of the weld treatment 0.2% 1.0% strength (L0=5d0) in J CVN
N/mm2 N/mm2 N/mm2 %
metal according
to EN 1597-1 AW 450 500 650 8
(min. values at RT)

Structure Austenite

Welding instruction
Materials Preheating Postweld heat treatment
Matching/similar None None
cast steel grades

Polarity = –
Shielding gas (EN 439) I1

Approvals Controlas (0637)

Packaging and Diam. x Length (mm) kg / pack


weights 2.0 x 1000 10
2.4 x 1000 10
3.2 x 1000 10
Böhler Thyssen Schweisstechnik Deutschland GmbH – 09_2005 215