Production Technology of EPSBR

SBR1739N Product Standard

No. Indexes Min. Max.


1 Bound styrene, % 38.5 41.5
2 Volatile, % - 0.50
3 Ash, % - 0.40
4 Soap content, % - 0.50
5 Organic acid, % 3.90 5.70
6 Oil content, % 25.3 29.3
100℃
7 Mooney viscosity of raw rubber, ML1+4 47 57
25min 7.4 11.3
300% tensile stress at a given
8 35min 9.3 13.2
elongation (145℃ ×), MPa
50min 10.8 14.7
9 Tensile strength (145℃ ×35min), MPa 18.6 (190) -
10 Elongation at break (145℃ ×35min), % 420 -