New Shine Technology Serial No.

FY 2022-23
Customer's
Our Challan - 5782

NST Plot No. 101, HSIDC, Kutana , Hisar Road,


Rohtak (Haryana) India
Date - P06/10/2022
Challan No. 1180

Date - 03/10/2022 Date - 06/10/2022


Pin : 124001

PRE-DISPATCH INSPECTION REPORT


Customer's Name & Address - Part No. 90107-K0L-D000 Qty. - 533.0 Kgs

M/s Shri Prabhu Fastners Part Name - BOLT SPL M6X16 Mat. Received Date - 03/10/2022

Plot No. 169 old IDC Colony Hissar Road ,Rohtak


Operation - MFZn. Ni1 - B (Zinc Nickel Plating ) Production Date - 03/10/2022
…………………………………………………………
MEASURING OPSERVATIONS
S.N. PARAMETER SPECIFICATION JUDGEMENT
INSTRUMENT 1 2 3 4 5
Should be free from Dent ,
1 Appearance Rust , Pitted & other Visual OK OK OK OK OK OK
Handaling Defecats

MFZn. Ni1 - B
2 Surface Finish (Zinc Nickel Plating ) Visual OK OK OK OK OK OK

6~10µ Plating Thickness


3 Plating Thickness
Tester
10.6µ 9.4µ 8.3µ 9.1µ 10.2µ OK

Nickle % should be N/A


12% to 16%
SRF Ni% N/A
%
4
Zinc / Nickle Nickle % should be
Machine Zi% Found 7~9 % OK
06% to 10%
Digital Time & Temp. ……… ……… ……… ……… ………
5 Hydrogen Embrittilement At 210C0 - 230C0 in 8 Hrs.
Controller
N/A

Digital Time & Temp. 20 Minutes


6 Baking At 60-80 0C Temp
Controller
OK

7 Open Air Curing 24 Hrs. Min. Clock (From - 03/10/2022 To - 06/10/2022 OK

White Rust……….hrs. Red


8 SST Life
Rust………….hrs
SST Chamber OK

Remarks

Result
Prepaired By - Approved By -
Our Challan - 10104
New Shine Technology Serial No. FY 2024-2025
Customer's

NST Plot No. 101, HSIDC, Kutana , Hisar Road,


Rohtak (Haryana) India
Date - 22/05/2024
Challan No. 360

Date - 21/05/2024 Date - 22/05/2024


Pin : 124001

PRE-DISPATCH INSPECTION REPORT


Customer's Name & Address - Part No.:- 81255-K0YA-D000 Qty. - 10.30 Kgs

M/s Shri Prabhu Fastners Part Name:- COLLAR LUGGAGE BOX Mat. Received Date - 21/05/2024

Plot No. 169 old IDC Colony Hissar Road ,Rohtak


Operation - MFZn2-C (AS PER HES D2003-03) Production Date - 22/05/2024

S.N. PARAMETER SPECIFICATION INSPECTION METHOD OBSERVATIONS PART PHOTO

1 Peeling not Allowed Part found free from Peel off


2 Blisters not allowed Part found free from Blisters
3 Pin holes not allowed Part found free from Pin holes
4 Exposed base note allowed Part found free from Expossed base
Exposed nickel (or copper) not
5 Coating found free from Expossed Nickel and copper
allowed
6 Pitting not Allowed Part found free from Pitting
7 Rough surfaces not Allowed Part found free from rough Surface
8 Stains not Allowed Part found free from Stains
9 Spot not Allowed Part found free from Spot
10 Blushing not Allowed Part found free from Blushing
11 Appearance
Burning not Allowed Visually
Part found free from Burning
12 Clouding not Allowed Part found free from Clouding
13 Wrinkles not Allowed Part found free from Wrinkles
14 Uneven surface not Allowed Part found free from Uneven surface
15 Polishing marks not Allowed Part found free from Polishing marks
Deformation due to plating not
16 Part found free from Deformation
Allowed
Flawas of base material surface not
17 Part found free from Flaws of base material surface
Allowed
18 Dent not Allowed Part found free from Dent
19 Scratches not Allowed Part found free from Scratches
20 Uneven color not Allowed Part found free from Uneven color
Remarks

Prepaired By - Approved By -