Butyl rubber
PHYSICAL PROPERTIES
(1) Mooney Viscosity testing in accordance with ASTM D1646, MV2000, unamassed sample.
(2) Rheometer testing in accordance with ASTM D2084. Temp. 160°C, Frequency 100 cpm,30 mins. test, 3°Arc.
(3) Characteristics determined on a standard compound of the following formulation; in accordance with
ASTM D3568 Reprocessed 1675 100
HAF N330 IRB7 50
Zinc Oxide 3
Stearic Acid 1
TMTD 1
Sulfur 1.75
(4) Press cure: 40 mins. at 150°C
TYPICAL RHEOMETER TEST
Applications Tires and Tubes, Sealants, Tank Linings along with a any other
Industrial and Mechanical application which requires low gas
permeability and chemical inertness.
Packaging 25 kg bale wrapped in EVA film of melting point not more than 75°C
is further packed either in appropriate bulk packing (metal
container) or as individual bale in PP bag.
Disclaimer: The results were obtained under standard experimental conditions. No warranty is given if the
experimental conditions and procedures are changed. Therefore, it is highly essential that you test our product
and information to evaluate to your own satisfaction whether they are suitable for your intended use and
applications. All information are given without warranty or guarantee and is subject to change without notice.
Note: The information contained in this publication is current as of Feb 16, 2024. Please contact 2M Elastomers to determine if this publication has been revised
Head Office: Rustom Building, 3rd Floor, 29 Veer Nariman Road,400001, Mumbai (MH) Phone :+91-22-22881293,94605-64889 Pankaj Baid
Unit I: Plot No.711 & 711/1, Phase III , GIDC, Umbergaon- 396171, Valsad (Gujrat)Unit II :Plot No. 1229 & 1230, Phase I, Sarigam- 396155,
Valsad (Gujrat) email: info@nishigandhapolymers.com , pawan@nishigandhapolymers.com