<Blade KSPB2026>

semi product after grind-


ing and heat treatment
Heat treatment
Raw Material Semi-product (vacuum) grinding
HRC_45~50 (Target 48)

Pocket cutting Pocket cutting


Blackening Deburring
(Form endmill) (Rough)

1.Slotting saw, wire cutting, end_mill cutting


it is depend on “V” area size (Tip seat area)
->you can cutting there with End mill also (not hard to cutting)
mostly we are using end mill bcz of cost

2. As you know well, you need to cut there as much as possible before start
Laser marking cut there with form endmill (blue line area_on left pic)